Fundamentals of Nanoindentation and Nanotribology IV
Herausgeber: Le Bourhis, Eric
Fundamentals of Nanoindentation and Nanotribology IV
Herausgeber: Le Bourhis, Eric
- Gebundenes Buch
Andere Kunden interessierten sich auch für
- MEMS and Nanotechnology, Volume 5147,99 €
- Microelectromechanical Systems - Materials and Devices IV37,99 €
- Micro-Nanoindentation in Materials Science151,99 €
- Nanotribology and Nanomechanics75,99 €
- Fellah MamounLe Ti-6Al-4Fe et ses applications aux biomatériaux62,99 €
- Holger WorrackMiniaturmessverfahren insbesondere Nanoindentation zur Bestimmung von Materialparametern bei kleinen Werkstoffmengen36,10 €
- Carmen Müller-Karger / Sara Wong / Alexandra La Cruz (eds.)IV Latin American Congress on Biomedical Engineering 2007, Bioengineering Solutions for Latin America Health, September 24th-28th, 2007, Margarita Island, Venezuela231,99 €
-
-
-
Produktdetails
- Verlag: Cambridge University Press
- Seitenzahl: 200
- Erscheinungstermin: 15. Mai 2008
- Englisch
- Abmessung: 235mm x 157mm x 15mm
- Gewicht: 450g
- ISBN-13: 9781558999893
- ISBN-10: 1558999892
- Artikelnr.: 35485882
Preface; Acknowledgments; Part I. Nanomechanics, Tribology and
Nanostructures: 1. Comprehensive mechanical and tribological
characterization of ultra-thin-films Norm Gitis, Michael Vinogradov, Ilja
Hermann and Suresh Kuiry; 2. Mechanical response of a single and released
InP membrane Eric Le Bourhuis and Gilles Patriarche; 3. Indentation
response of nanostructured turfs A. A. Zbib, S. Dj. Mesarovic, D. F. Bahr,
E. T. Lilleodden, J. Jiao and D. McClain; 4. Effect of hydrostatic pressure
on indentation modulus W. M. Mook and W. W. Gerberich; Part II. Size
Effects and Indentation of Thin Films: 5. Microstructural investigation of
the deformation zone below nano-indents in copper Martin Rester, Christian
Motz and Reinhard Pippan; 6. Microstructure and mechanical properties
characterization of nanocrystalline copper films Nursiani Indah Tjahyono
and Yu Lung Chiu; 7. Mechanical properties of 3C-SiC films for MEMS
applications Jayadeep Deva Reddy, Alex A. Volinsky, Christopher L. Frewin,
Chris Locke and Stephen E. Sandow; 8. Strength measurement in brittle thin
films Oscar Borrero-Lopez, Mark Hoffman, Avi Bendavid and Phil J. Martin;
Part III. Nanotribology and Friction: 9. Measurement of ultrathin film
mechanical properties by integrated nano-scratch/indentation approach
Ashraf Bastawros, Wei Che and Abhijit Chandra; 10. Theory of lubrication
due to poly-electrolyte polymer brushes Jeffrey B. Sokoloff; 11.
Tip-induced calcite single crystal nanowear Ramakrishna Gunda and Alex A.
Volinsky; 12. Study on the damage mechanisms in WC-Co hard metals during
scratch testing Siphilisiwe Mdlovu, Karsten Durst, Heinz Werner Hoeppel and
Mathias Goeken; Part IV. Modeling, Simulation and Analysis of Indentation
Data: 13. Mapping of the initial volume at the onset of plasticity in
nanoindentation T. T. Zhu, K. M. Y. P'ng, M. Hopkinson, A. J. Bushby and D.
J. Dunstan; 14. Quasi-static and oscillatory indentation in linear
viscoelastic solids Yang-Tse Cheng and Che-Min Cheng; 15. Indentation of
nonlinearly viscoelastic solids Michaelle L. Oyen; 16. Determination of
residual stress and yield stress simultaneously by indentation method with
dual indenters Baoxing Xu, Xinmei Wang and Zhufeng Yue; 17. Instrumented
indentation contact with sharp probes of varying acuity Dylan J. Morris;
18. An algorithm to determine the plastic properties of materials based on
the loading data in single sharp indentation Akio Yonezu, Hiroyuki Hirakata
and Kohji Minoshima; 19. Plasticity characteristics obtained through
instrumental indentation Yuliy Milman, Sergey Dub and Alex Golubenko; 20.
Nanoindentation analysis of plasticity evolution during spherical
microindentation of bulk metallic glass Byung-Gil Yoo and Jae-il Jang; 21.
Reverse plasticity in nanindentation Yongjiang Huang, Nursiani Indah
Tjahyono, Jun Shen and Yu Lung Chiu; 22. Uniaxial compression behavior of
bulk nano-twinned gold from moecular dynamics simulation Chuang Deng and
Frederic Sansoz; Part V. Nonomechanics of Polymers, Time Dependent
Characterization: 23. Interfacial characterization of multiple layer
coatings on thermoplastic olefins (TPO) Aaron M. Forster, Chris A.
Michaels, Justin Lucas and Lipiin Sung; 24. Viscoelastic behavior of a
centrally loaded circular film being clamped at the circumference Michaelle
L. Oyen, Kuo-kang Liu and Kai-tak Wan; 25. Analysis of indentation creep D.
S. Stone and A. A. Elmustafa; 26. Haasen plot activation analysis of
constant-force indentation creep in FCC systems Vineet Bhakhri and Robert
J. Klassen; 27. Mechanical properties of sputtered silicon oxynitride films
by nanoindentation Yan Liu, I-Kuan Lin and Xin Zhang; Author index; Subject
index.
Nanostructures: 1. Comprehensive mechanical and tribological
characterization of ultra-thin-films Norm Gitis, Michael Vinogradov, Ilja
Hermann and Suresh Kuiry; 2. Mechanical response of a single and released
InP membrane Eric Le Bourhuis and Gilles Patriarche; 3. Indentation
response of nanostructured turfs A. A. Zbib, S. Dj. Mesarovic, D. F. Bahr,
E. T. Lilleodden, J. Jiao and D. McClain; 4. Effect of hydrostatic pressure
on indentation modulus W. M. Mook and W. W. Gerberich; Part II. Size
Effects and Indentation of Thin Films: 5. Microstructural investigation of
the deformation zone below nano-indents in copper Martin Rester, Christian
Motz and Reinhard Pippan; 6. Microstructure and mechanical properties
characterization of nanocrystalline copper films Nursiani Indah Tjahyono
and Yu Lung Chiu; 7. Mechanical properties of 3C-SiC films for MEMS
applications Jayadeep Deva Reddy, Alex A. Volinsky, Christopher L. Frewin,
Chris Locke and Stephen E. Sandow; 8. Strength measurement in brittle thin
films Oscar Borrero-Lopez, Mark Hoffman, Avi Bendavid and Phil J. Martin;
Part III. Nanotribology and Friction: 9. Measurement of ultrathin film
mechanical properties by integrated nano-scratch/indentation approach
Ashraf Bastawros, Wei Che and Abhijit Chandra; 10. Theory of lubrication
due to poly-electrolyte polymer brushes Jeffrey B. Sokoloff; 11.
Tip-induced calcite single crystal nanowear Ramakrishna Gunda and Alex A.
Volinsky; 12. Study on the damage mechanisms in WC-Co hard metals during
scratch testing Siphilisiwe Mdlovu, Karsten Durst, Heinz Werner Hoeppel and
Mathias Goeken; Part IV. Modeling, Simulation and Analysis of Indentation
Data: 13. Mapping of the initial volume at the onset of plasticity in
nanoindentation T. T. Zhu, K. M. Y. P'ng, M. Hopkinson, A. J. Bushby and D.
J. Dunstan; 14. Quasi-static and oscillatory indentation in linear
viscoelastic solids Yang-Tse Cheng and Che-Min Cheng; 15. Indentation of
nonlinearly viscoelastic solids Michaelle L. Oyen; 16. Determination of
residual stress and yield stress simultaneously by indentation method with
dual indenters Baoxing Xu, Xinmei Wang and Zhufeng Yue; 17. Instrumented
indentation contact with sharp probes of varying acuity Dylan J. Morris;
18. An algorithm to determine the plastic properties of materials based on
the loading data in single sharp indentation Akio Yonezu, Hiroyuki Hirakata
and Kohji Minoshima; 19. Plasticity characteristics obtained through
instrumental indentation Yuliy Milman, Sergey Dub and Alex Golubenko; 20.
Nanoindentation analysis of plasticity evolution during spherical
microindentation of bulk metallic glass Byung-Gil Yoo and Jae-il Jang; 21.
Reverse plasticity in nanindentation Yongjiang Huang, Nursiani Indah
Tjahyono, Jun Shen and Yu Lung Chiu; 22. Uniaxial compression behavior of
bulk nano-twinned gold from moecular dynamics simulation Chuang Deng and
Frederic Sansoz; Part V. Nonomechanics of Polymers, Time Dependent
Characterization: 23. Interfacial characterization of multiple layer
coatings on thermoplastic olefins (TPO) Aaron M. Forster, Chris A.
Michaels, Justin Lucas and Lipiin Sung; 24. Viscoelastic behavior of a
centrally loaded circular film being clamped at the circumference Michaelle
L. Oyen, Kuo-kang Liu and Kai-tak Wan; 25. Analysis of indentation creep D.
S. Stone and A. A. Elmustafa; 26. Haasen plot activation analysis of
constant-force indentation creep in FCC systems Vineet Bhakhri and Robert
J. Klassen; 27. Mechanical properties of sputtered silicon oxynitride films
by nanoindentation Yan Liu, I-Kuan Lin and Xin Zhang; Author index; Subject
index.
Preface; Acknowledgments; Part I. Nanomechanics, Tribology and
Nanostructures: 1. Comprehensive mechanical and tribological
characterization of ultra-thin-films Norm Gitis, Michael Vinogradov, Ilja
Hermann and Suresh Kuiry; 2. Mechanical response of a single and released
InP membrane Eric Le Bourhuis and Gilles Patriarche; 3. Indentation
response of nanostructured turfs A. A. Zbib, S. Dj. Mesarovic, D. F. Bahr,
E. T. Lilleodden, J. Jiao and D. McClain; 4. Effect of hydrostatic pressure
on indentation modulus W. M. Mook and W. W. Gerberich; Part II. Size
Effects and Indentation of Thin Films: 5. Microstructural investigation of
the deformation zone below nano-indents in copper Martin Rester, Christian
Motz and Reinhard Pippan; 6. Microstructure and mechanical properties
characterization of nanocrystalline copper films Nursiani Indah Tjahyono
and Yu Lung Chiu; 7. Mechanical properties of 3C-SiC films for MEMS
applications Jayadeep Deva Reddy, Alex A. Volinsky, Christopher L. Frewin,
Chris Locke and Stephen E. Sandow; 8. Strength measurement in brittle thin
films Oscar Borrero-Lopez, Mark Hoffman, Avi Bendavid and Phil J. Martin;
Part III. Nanotribology and Friction: 9. Measurement of ultrathin film
mechanical properties by integrated nano-scratch/indentation approach
Ashraf Bastawros, Wei Che and Abhijit Chandra; 10. Theory of lubrication
due to poly-electrolyte polymer brushes Jeffrey B. Sokoloff; 11.
Tip-induced calcite single crystal nanowear Ramakrishna Gunda and Alex A.
Volinsky; 12. Study on the damage mechanisms in WC-Co hard metals during
scratch testing Siphilisiwe Mdlovu, Karsten Durst, Heinz Werner Hoeppel and
Mathias Goeken; Part IV. Modeling, Simulation and Analysis of Indentation
Data: 13. Mapping of the initial volume at the onset of plasticity in
nanoindentation T. T. Zhu, K. M. Y. P'ng, M. Hopkinson, A. J. Bushby and D.
J. Dunstan; 14. Quasi-static and oscillatory indentation in linear
viscoelastic solids Yang-Tse Cheng and Che-Min Cheng; 15. Indentation of
nonlinearly viscoelastic solids Michaelle L. Oyen; 16. Determination of
residual stress and yield stress simultaneously by indentation method with
dual indenters Baoxing Xu, Xinmei Wang and Zhufeng Yue; 17. Instrumented
indentation contact with sharp probes of varying acuity Dylan J. Morris;
18. An algorithm to determine the plastic properties of materials based on
the loading data in single sharp indentation Akio Yonezu, Hiroyuki Hirakata
and Kohji Minoshima; 19. Plasticity characteristics obtained through
instrumental indentation Yuliy Milman, Sergey Dub and Alex Golubenko; 20.
Nanoindentation analysis of plasticity evolution during spherical
microindentation of bulk metallic glass Byung-Gil Yoo and Jae-il Jang; 21.
Reverse plasticity in nanindentation Yongjiang Huang, Nursiani Indah
Tjahyono, Jun Shen and Yu Lung Chiu; 22. Uniaxial compression behavior of
bulk nano-twinned gold from moecular dynamics simulation Chuang Deng and
Frederic Sansoz; Part V. Nonomechanics of Polymers, Time Dependent
Characterization: 23. Interfacial characterization of multiple layer
coatings on thermoplastic olefins (TPO) Aaron M. Forster, Chris A.
Michaels, Justin Lucas and Lipiin Sung; 24. Viscoelastic behavior of a
centrally loaded circular film being clamped at the circumference Michaelle
L. Oyen, Kuo-kang Liu and Kai-tak Wan; 25. Analysis of indentation creep D.
S. Stone and A. A. Elmustafa; 26. Haasen plot activation analysis of
constant-force indentation creep in FCC systems Vineet Bhakhri and Robert
J. Klassen; 27. Mechanical properties of sputtered silicon oxynitride films
by nanoindentation Yan Liu, I-Kuan Lin and Xin Zhang; Author index; Subject
index.
Nanostructures: 1. Comprehensive mechanical and tribological
characterization of ultra-thin-films Norm Gitis, Michael Vinogradov, Ilja
Hermann and Suresh Kuiry; 2. Mechanical response of a single and released
InP membrane Eric Le Bourhuis and Gilles Patriarche; 3. Indentation
response of nanostructured turfs A. A. Zbib, S. Dj. Mesarovic, D. F. Bahr,
E. T. Lilleodden, J. Jiao and D. McClain; 4. Effect of hydrostatic pressure
on indentation modulus W. M. Mook and W. W. Gerberich; Part II. Size
Effects and Indentation of Thin Films: 5. Microstructural investigation of
the deformation zone below nano-indents in copper Martin Rester, Christian
Motz and Reinhard Pippan; 6. Microstructure and mechanical properties
characterization of nanocrystalline copper films Nursiani Indah Tjahyono
and Yu Lung Chiu; 7. Mechanical properties of 3C-SiC films for MEMS
applications Jayadeep Deva Reddy, Alex A. Volinsky, Christopher L. Frewin,
Chris Locke and Stephen E. Sandow; 8. Strength measurement in brittle thin
films Oscar Borrero-Lopez, Mark Hoffman, Avi Bendavid and Phil J. Martin;
Part III. Nanotribology and Friction: 9. Measurement of ultrathin film
mechanical properties by integrated nano-scratch/indentation approach
Ashraf Bastawros, Wei Che and Abhijit Chandra; 10. Theory of lubrication
due to poly-electrolyte polymer brushes Jeffrey B. Sokoloff; 11.
Tip-induced calcite single crystal nanowear Ramakrishna Gunda and Alex A.
Volinsky; 12. Study on the damage mechanisms in WC-Co hard metals during
scratch testing Siphilisiwe Mdlovu, Karsten Durst, Heinz Werner Hoeppel and
Mathias Goeken; Part IV. Modeling, Simulation and Analysis of Indentation
Data: 13. Mapping of the initial volume at the onset of plasticity in
nanoindentation T. T. Zhu, K. M. Y. P'ng, M. Hopkinson, A. J. Bushby and D.
J. Dunstan; 14. Quasi-static and oscillatory indentation in linear
viscoelastic solids Yang-Tse Cheng and Che-Min Cheng; 15. Indentation of
nonlinearly viscoelastic solids Michaelle L. Oyen; 16. Determination of
residual stress and yield stress simultaneously by indentation method with
dual indenters Baoxing Xu, Xinmei Wang and Zhufeng Yue; 17. Instrumented
indentation contact with sharp probes of varying acuity Dylan J. Morris;
18. An algorithm to determine the plastic properties of materials based on
the loading data in single sharp indentation Akio Yonezu, Hiroyuki Hirakata
and Kohji Minoshima; 19. Plasticity characteristics obtained through
instrumental indentation Yuliy Milman, Sergey Dub and Alex Golubenko; 20.
Nanoindentation analysis of plasticity evolution during spherical
microindentation of bulk metallic glass Byung-Gil Yoo and Jae-il Jang; 21.
Reverse plasticity in nanindentation Yongjiang Huang, Nursiani Indah
Tjahyono, Jun Shen and Yu Lung Chiu; 22. Uniaxial compression behavior of
bulk nano-twinned gold from moecular dynamics simulation Chuang Deng and
Frederic Sansoz; Part V. Nonomechanics of Polymers, Time Dependent
Characterization: 23. Interfacial characterization of multiple layer
coatings on thermoplastic olefins (TPO) Aaron M. Forster, Chris A.
Michaels, Justin Lucas and Lipiin Sung; 24. Viscoelastic behavior of a
centrally loaded circular film being clamped at the circumference Michaelle
L. Oyen, Kuo-kang Liu and Kai-tak Wan; 25. Analysis of indentation creep D.
S. Stone and A. A. Elmustafa; 26. Haasen plot activation analysis of
constant-force indentation creep in FCC systems Vineet Bhakhri and Robert
J. Klassen; 27. Mechanical properties of sputtered silicon oxynitride films
by nanoindentation Yan Liu, I-Kuan Lin and Xin Zhang; Author index; Subject
index.