In this thesis, LMD is applied to produce ultrafine TiC particle reinforced Inconel 625 composite parts. The effects of laser energy input per unit length (LEIPUL) on microstructure development, densification response, and mechanical performance including wear performance and tensile properties are comprehensively studied.

Produktbeschreibung
In this thesis, LMD is applied to produce ultrafine TiC particle reinforced Inconel 625 composite parts. The effects of laser energy input per unit length (LEIPUL) on microstructure development, densification response, and mechanical performance including wear performance and tensile properties are comprehensively studied.