The 14th International Symposium on Superalloys (Superalloys 2020) highlights technologies for lifecycle improvement of superalloys. In addition to the traditional focus areas of alloy development, processing, mechanical behavior, coatings, and environmental effects, this volume includes contributions from academia, supply chain, and product-user members of the superalloy community that highlight technologies that contribute to improving manufacturability, affordability, life prediction, and performance of superalloys.
The 14th International Symposium on Superalloys (Superalloys 2020) highlights technologies for lifecycle improvement of superalloys. In addition to the traditional focus areas of alloy development, processing, mechanical behavior, coatings, and environmental effects, this volume includes contributions from academia, supply chain, and product-user members of the superalloy community that highlight technologies that contribute to improving manufacturability, affordability, life prediction, and performance of superalloys.Hinweis: Dieser Artikel kann nur an eine deutsche Lieferadresse ausgeliefert werden.
Sammy Tin, Illinois Institute of Technology, Chicago, IL 60616; Mark Hardy, Rolls-Royce plc, Derby, Derbyshire, UK DE24 8BJ; Justin Clews, PCC Structurals, Portland, OR 97206; Jonathan Cormier, ISAE-ENSMA, Futuroscope Chasseneuil, France 86961; Qiang Charles Feng, University of Science and Technology Beijing, Beijing, China 100083; John Marcin, Collins Aerospace, Windsor Locks, CT 06096; Chris O'Brien, ATI Specialty Materials, Monroe, NC 28110; Akane Suzuki, GE Global Research, Niskayuna, NY 12309
Inhaltsangabe
Advanced Modeling Tools for Processing and Lifing of Aeroengine Components.- Developing Alloy Compositions for Future High Temperature Disk Rotors.- Development of AGAT, a 3rd Generation Nickel Based Superalloy for Single Crystal Turbine Blade Applications.- Segregation of solutes at dislocations: A new alloy design parameter for advanced superalloys.- Ni-Co-based Wrought Superalloys Containing High W - Microstructure Design for a Balance of Properties.- On the influence of alloy composition on creep behavior of single crystal (SX) Ni-based superalloys.- Platinum containing new generation nickel-based superalloy for single crystalline applications.- Development and Application of New Cast & Wrought Ni-base Superalloy M647 for Turbine Disk.- Alloy Design and Microstructural Evolution during Heat Treatment of Newly Developed Cast & Wrought Ni-base Superalloy M647 for Turbine Disk Application.- Thermodynamic Simulation and Experimental Validation of Phase Stability in Ni-based Superalloys.
Advanced Modeling Tools for Processing and Lifing of Aeroengine Components.- Developing Alloy Compositions for Future High Temperature Disk Rotors.- Development of AGAT, a 3rd Generation Nickel Based Superalloy for Single Crystal Turbine Blade Applications.- Segregation of solutes at dislocations: A new alloy design parameter for advanced superalloys.- Ni-Co-based Wrought Superalloys Containing High W - Microstructure Design for a Balance of Properties.- On the influence of alloy composition on creep behavior of single crystal (SX) Ni-based superalloys.- Platinum containing new generation nickel-based superalloy for single crystalline applications.- Development and Application of New Cast & Wrought Ni-base Superalloy M647 for Turbine Disk.- Alloy Design and Microstructural Evolution during Heat Treatment of Newly Developed Cast & Wrought Ni-base Superalloy M647 for Turbine Disk Application.- Thermodynamic Simulation and Experimental Validation of Phase Stability in Ni-based Superalloys.
Es gelten unsere Allgemeinen Geschäftsbedingungen: www.buecher.de/agb
Impressum
www.buecher.de ist ein Internetauftritt der buecher.de internetstores GmbH
Geschäftsführung: Monica Sawhney | Roland Kölbl | Günter Hilger
Sitz der Gesellschaft: Batheyer Straße 115 - 117, 58099 Hagen
Postanschrift: Bürgermeister-Wegele-Str. 12, 86167 Augsburg
Amtsgericht Hagen HRB 13257
Steuernummer: 321/5800/1497
USt-IdNr: DE450055826